Quantcast
  1. This site uses cookies. By continuing to use this site, you are agreeing to our use of cookies. Learn More.

Tempilaq--How Much

Discussion in 'Handloading and Reloading' started by j2crows, Sep 28, 2011.

Thread Status:
Not open for further replies.
  1. j2crows

    j2crows Member

    Joined:
    Feb 27, 2011
    Messages:
    177
    Location:
    New Mexico
    Which of these 3 cases do you think shows the correct amount of Tempilaq?
     

    Attached Files:

  2. Sport45

    Sport45 Member

    Joined:
    Mar 5, 2004
    Messages:
    2,783
    Location:
    Houston, TX
    I'd say the middle one. But shouldn't it be on the outside and a across the shoulder?
     
  3. dave from mesa

    dave from mesa Member

    Joined:
    Mar 6, 2008
    Messages:
    280
    Location:
    Mesa, AZ
  4. Hondo 60
    • Contributing Member

    Hondo 60 Member

    Joined:
    Sep 6, 2009
    Messages:
    5,381
    Location:
    Manitowoc, WI
    dave from mesa - it's for annealing - here's a You Tube link to help you understand.
    (I didn't know either so I had to google it)

    Induction Annealing with Tempilaq

    http://www.youtube.com/watch?v=Uasv-Pyxu4g
     
  5. MEHavey

    MEHavey Member

    Joined:
    Jul 27, 2010
    Messages:
    2,399
    Location:
    virginia
    I believe 750ᵒF Tempilaq is blue (and would be normally used right inside the neck). What temp is that yellow?

    (But) assuming that's 750-ish fluid any of the cases would be fine as you're just looking for melt/color change. (In fact the one on the left would be the most efficient use of the fluid)

    If using 475-500ᵒF Tempilaq, it would go on the case body 1/4" below the shoulder.
     
    Last edited: Sep 29, 2011
  6. j2crows

    j2crows Member

    Joined:
    Feb 27, 2011
    Messages:
    177
    Location:
    New Mexico
    650 degrees
     