RSVP2RIP
Member
Is anyone using this and having good results? I've cast for muzzleloader for years and I'm going to start for .38 spl. I'd like to stay with alloys that have only lead and tin in them because plumbers lead and 50/50 solder are free to me, kinda. I don't know where I could get antimony around here (other than in 95/5 solder) without ordering it, which I imagine shipping is expensive. I heard that having high tin in the alloy causes the bullet to soften over time, is there any truth to this?