BigMacMI
Member
- Joined
- Nov 17, 2016
- Messages
- 127
I got the 30# F.A.R.T. I have run probably 6 batches of cases through thus far. Using Armoral Wash n Wax for soap, and Lemishine powder.
I have been experimenting with times and volume of Lemi. From 1-4 45ACP cases worth.
Everything has been coming out really dull (one batch was too long I think because it turned an olive color).
Cases are clean enough to reload and shoot, but not very shiny.
I did just finish a batch of .223 which I used the small packet of solution that F.A. sends as a sample with the FART. Super shiny and clean. Leads me to believe that it is more of a solution issue in my mix.
Problem is, I only have 1 more batch of dirty brass to run (unless i can re-run some of the dull ones to experiment on getting them shiny).
Has anyone figured out the ratios for the F.A. solution? (it was blue).
I have been experimenting with times and volume of Lemi. From 1-4 45ACP cases worth.
Everything has been coming out really dull (one batch was too long I think because it turned an olive color).
Cases are clean enough to reload and shoot, but not very shiny.
I did just finish a batch of .223 which I used the small packet of solution that F.A. sends as a sample with the FART. Super shiny and clean. Leads me to believe that it is more of a solution issue in my mix.
Problem is, I only have 1 more batch of dirty brass to run (unless i can re-run some of the dull ones to experiment on getting them shiny).
Has anyone figured out the ratios for the F.A. solution? (it was blue).